MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory GV-2 FWA black 9225 is used for injection molding technical parts, exhibiting exceptional characteristics even after moisture absorption:
  • high stiffness and strength
  • dimensional stability, low warpage
  • good chemical resistance
  • good surface finish
Grivory GV is the economical alternative to die-cast alloys. Grivory GV-2 FWA black 9225 is a specially heat stabilized material. It is particularly suitable for parts in direct contact with drinking water and food. Grivory GV-2 FWA black 9225 is suitable for all engineering thermoplastic applications with the requirement of approvals in contact with foodstuffs or/and in contact with drinking water.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccDry; ISO 1183
Water Absorption 5.0 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 200 MPaConditioned; ISO 2039-1
 225 MPaDry; ISO 2039-1
Tensile Strength at Break 125 MPaConditioned; ISO 527-1/-2
 145 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 4.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 7200 MPaConditioned; ISO 527-1/-2
 8200 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 33.0 kV/mmDry; IEC 60243-1
 33.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 575 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °CLong Term; ISO 2578
 220 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 65.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sanitary, water and gas supply
ProcessingInjection Molding
Product AttributesPartially aromatic Polyamide
Water ContactACS
 DVGW W270
 KTW
 NSF 61
 WRAS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Techmer ES HiFill® PC GF20 20% Glass Filled
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60
BASF Ultramid® C33L 01 PA66/6 (Dry)

PGRH322 / 157031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.