MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) FOMBLIN® LC55 PFPE Lubricant  (Unverified Data**)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requiring low viscosity.

Information provided by Solvay Solexis, Inc.

Key Words: Perfluorinated Polyether
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.87 g/cc0.0676 lb/in³ASTM D891
Viscosity Measurement 9292Viscosity Index; ASTM D2270
Kinematic Viscosity 53 cSt
@Temperature 20.0 °C
53 cSt
@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 21.5 cSt21.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 4.2 cSt4.2 cStASTM D445
Molecular Weight 1700 g/mol1700 g/mol
Evaporation Loss 2.5 %2.5 %22 hrs. at 60°C; ASTM 2595
 40 %40 %22 hrs. at 120°C; ASTM 2595
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 100 kg221 lb (mass)Mean Hertz Load; IP 239
 400 kg882 lb (mass)Welding Load; IP 239
Four Ball Wear 0.600 mm0.0236 inAvg. scar diameter; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -56.0 °C-68.8 °FASTM D97
 
Descriptive Properties
Approximate ISO Grade22
Oxygen Impact (BAM) 100°C, Impact Pressure160 atm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WAUSI28 / 74587

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.