LNP LUBRICOMP RL0049S compound is based on Nylon 6/6 resin containing 20% PTFE. Added features of this grade include: Flame Retardant, Heat Stabilized, Wear Resistant. Features: Flame Retardant,Wear resistant,Heat Stabilized Information provided by SABIC |