MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R433H BK0746 PA66-I-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Vydyne R433H BK0746 is designed to reinforce downgauged steel and aluminum used in vehicle body-in-white (BIW) structures, helping reduce weight without sacrificing safety or comfort.R433H BK0746 has improved energy absorption over traditional glass-filled PA66, helping reduce noise, vibration and harshness (NVH) and absorbing impact energy from crashes. Using R433H BK0746 in the BIW structure reinforces sheet metal, helping manufacturers shave substantial weight and improve efficiency. Trends in lightweight and NVH are becoming even more paramount with the growth of Electric Vehicles. Vydyne R433H BK0746 has excellent performance attributes to support applications where this will be of prime importance such as battery frames and housings.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccDAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 102 MPa50% RH; ISO 527-2
 151 MPaDAM; ISO 527-2
Tensile Strength, Yield 103 MPa50% RH; ISO 527-2
 150 MPaDAM; ISO 527-2
Elongation at Break 3.6 %DAM; ISO 527-2
 8.5 %50% RH; ISO 527-2
Elongation at Yield 3.3 %DAM; ISO 527-2
 7.4 %50% RH; ISO 527-2
Tensile Modulus 6200 MPa50% RH; ISO 527-2
 9600 MPaDAM; ISO 527-2
Flexural Strength 132 MPa50% RH; ISO 178
 215 MPaDAM; ISO 178
Flexural Modulus 6000 MPa50% RH; ISO 178
 8400 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 18.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 24.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 27.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 92.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 96.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 96.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 16.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 17.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 17.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 24.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 27.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 11.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 262 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °CUnannealed; 50% RH; ISO 75-2/B
 260 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 241 °CUnannealed; 50% RH; ISO 75-2/A
 245 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA016G33
 ASTM, D6779 PA016G33
AppearanceBlack
Automotive Material SpecificationChrysler MS-DB-41_CPN2735
FeaturesBalanced Stiffness/Toughness
 Chemical Resistant
 Gasoline Resistant
 Good Dimensional Stability
 Good Heat Resistance
 Good Rigidity
 Good Tensile Strength
 Good Toughness
 Impact Modified
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9294 / 287644

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.