System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SCG Chemicals EL-Lene™ H511W High Density Polyethylene Wire & Cable Grade
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
HDPE, Fiber Grade
Material Notes:
Key Characteristics:
Contains special metal deactivator, high mechanical properties, high speed extrusion
Recommended Applications:
Insulation of communication cables
Information provided by SCG Chemicals
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.949
g/cc
ASTM D1505
ESCR 10% Igepal®
>=
168
hour
@Temperature 50.0 °C
F0; ASTM D1693
Oxidative Induction Time (OIT)
>=
100
min
@Temperature 200 °C
ASTM D3895
Melt Flow
0.90
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
62
ASTM D2240
Tensile Strength at Break
33.0
MPa
ASTM D638
Tensile Strength, Yield
230
kg(f)/cm²
ASTM D638
Elongation at Break
>= 600 %
ASTM D638
Flexural Modulus
>=
8000
kg(f)/cm²
ASTM D790
Izod Impact, Notched
14.0
kg-cm/cm
@Temperature 23.0 °C
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
ASTM D257
Dielectric Constant
2.32
ASTM D1531
Dielectric Strength
20.0
kV/mm
ASTM D149
Dissipation Factor
0.000060
ASTM D1531
Thermal Properties
Original Value
Comments
Brittleness Temperature
<=
-75.0
°C
ASTM D746
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow HDPE 30460M High Density Polyethylene
Eastman M3006-P Polyethylene
Eastman M30036-P Polyethylene
Dow HDPE 38152M High Density Polyethylene
LyondellBasell Alathon® M5370WC High Density Polyethylene
PSCGC915 / 120669
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.