MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 330 E FR Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Stainless Steel Fiber

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D 792
Additive Loading 10 %Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9600 psiASTM D 638
Elongation at Break 4.0 - 6.0 %ASTM D 638
Tensile Modulus 450 ksiASTM D 638
Flexural Strength 16500 psiASTM D 790
Flexural Modulus 450 ksiASTM D 790
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 14.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10 ohm-cmASTM D 257
Surface Resistance <= 1e+05ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness 37 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 37 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 38 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 40 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 44 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 45 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 46 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 48 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 53 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 53 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 55 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 530 - 580 °F
Mold Temperature 160 - 250 °F
Drying Temperature 250 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PQZWA2881 / 91395

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.