MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M FC-1100 Acid Mist Suppressant
Categories: Fluid; Polymer; Thermoplastic; Fluoropolymer

Material Notes: 3M™ Acid Mist Suppressant FC-1100 is a fluorochemical additive that provides outstanding sulfuric acid mist suppression in the copper electrowinning tankhouse without the formation of a stable foam blanket at the surface of the electrowinning cell. FC-1100 suppressant can significantly reduce tankhouse acid mist levels when used alone or in conjunction with mechanical barriers, such as polypropylene macrospheres, with no adverse effects to either the solvent extraction or electrowinning process

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Solids Content 45 - 55 %Fluorochemical
Viscosity <= 100 cP
Surface Tension 35 dynes/cm30 ppm
 40 dynes/cm14 ppm
 45 dynes/cm6 ppm
 50 dynes/cm1 ppm
 
Processing PropertiesOriginal ValueComments
Moisture Content 45 - 55 %
 
Descriptive Properties
ColorLight Amber
FormLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alclad Aluminum 6061-T6, T651
Eagle Brass 110 EPT COPPER, 1/2 Hard
Aluminum 1100-O
Aluminum 384.0-F Die Casting Alloy
Aluminum 6061-O

PMM33038 / 167785

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.