MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crosspolimeri GETILAN GPE/150 LE-LS Crosslinkable Polythene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: GETILAN: is the trade-mark of our crosslinkable polythene.

GETILAN GPE/150 LE-LS: medium density chemically crosslinkable polythene compound for low voltage power cable insulation and sheathing. The LS type is faster on crosslink. It is a conveniently grafted polythene able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 PSF. Where and when anti-ageing and anti-copper functions are required, we suggest our type MAC/100 SCU or MAC/203 (less reactive type). REACTION BETWEEN GRAFTING AND CATALYST: These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5

Certify: BS 7655 GP8, IEC502 XLPE

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 15.0 MPaIEC 811
 16.2 MPa
@Temperature 127 °C,
Time 144000 sec
air bomb; IEC 811
 16.5 MPa
@Temperature 135 °C,
Time 605000 sec
Heat Ageing; IEC 811
Elongation at Break 500 %IEC 811
 425 %
@Temperature 135 °C,
Time 605000 sec
Heat Ageing; IEC 811
 480 %
@Temperature 127 °C,
Time 144000 sec
air bomb; IEC 811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmBS 6622
 
Processing PropertiesOriginal ValueComments
Zone 1 150 °C
Zone 2 170 °C
Zone 3 190 °C
Zone 4 210 °C
Die Temperature 260 °C
Head Temperature 230 °C
 
Descriptive Properties
Hot Set Test0Residual Value, IEC 60811
 0.3200°C - 20 N/cm2, IEC 60811
Water absorption0.7 mg/cm²24 h at 100°C, IEC 811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS115 / 294199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.