MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Firelite LW HS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Insulating raw material base. Hydraulic bond. A low lime, highly insulating concrete for service up to 1200°C/2200°F. Can be cast or gunned. Particularly recommended for applications where sulphur is evident in the fuel used.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.34 g/cc0.0484 lb/in³dried to 110°C
Grain Size <= 4000 µm<= 4000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 6.40 MPa928 psiCold Crushing Strength, MST
 7.80 MPa
@Treatment Temp. 815 °C
1130 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 9.80 MPa
@Treatment Temp. 110 °C
1420 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.290 W/m-K
@Temperature 200 °C
2.01 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.310 W/m-K
@Temperature 400 °C
2.15 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.340 W/m-K
@Temperature 600 °C
2.36 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.360 W/m-K
@Temperature 800 °C
2.50 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.390 W/m-K
@Temperature 1000 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 1830 °F
Maximum Service Temperature, Air <= 1320 °C<= 2410 °F
Shrinkage 1.5 %1.5 %MST
 0.20 %
@Treatment Temp. 815 °C
0.20 %
@Treatment Temp. 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 38.8 %38.8 %
CaO 11.8 %11.8 %
Fe2O3 6.9 %6.9 %
K2O+Na2O 1.3 %1.3 %Na2O + K2O
SiO2 37.6 %37.6 %
TiO2 1.1 %1.1 %
 
Descriptive Properties
Net Material Required (kg/m³)1250
Water Addition30% by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6390 / 203174

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.