Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agent Applications: Agricultural & industrial film CAS No. 25087-34-7 Information provided by LG Chemical |