MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative humidity. The material is self-extinguishing. UL-94 V-0 approved – File No. E222199

Applications: Engineering and insulation material in large rotating electrical machines and insulation cylinders in dry transformers.

Information provided by Elektro-Isola

Key Words: IEC/EN 61212-3-1 EP GC 23, NEMA LI FR-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/cc
@Thickness >=0.000 mm
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.030 %24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 350 MPa
@Diameter >=100 mm
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 230 MPa
@Temperature 23.0 °C,
Time 86400 sec
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 400 MPa
@Diameter <=100 mm
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+10 ohm
@Diameter 8.00 - 10.0 mm
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Constant 4.5
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 4.5
@Frequency 1e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
Dielectric Strength 10.0 kV/mm
@Thickness 3.00 mm
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
 2.00 kV/mm
@Diameter >=3.00 mm
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Dissipation Factor 0.010
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 0.010
@Frequency 1000 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 145 °C
@Thickness 3.00 mm,
Time 7.20e+7 sec
IEC 60695-11-10; IEC/EN 61212-2 7.1
Flammability, UL94 V-0
@Thickness 3.00 mm
IEC 60695-11-10; IEC/EN 61212-2 7.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets

PELEKT016 / 126892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.