MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals UDIMET® alloy D-979 Fe-Ni Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of intermetallic phases, the alloy combines corrosion resistance with excellent tensile and stress rupture strength.

Information Provided by Special Metals Corporation

Key Words: UNS N09979; AMS 5746
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  69.0 MPa
@Temperature 871 °C,
Time 3.60e+6 sec
10000 psi
@Temperature 1600 °F,
Time 1000 hour
 145 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
21000 psi
@Temperature 1500 °F,
Time 1000 hour
 250 MPa
@Temperature 760 °C,
Time 3.60e+6 sec
36300 psi
@Temperature 1400 °F,
Time 1000 hour
 380 MPa
@Temperature 704 °C,
Time 3.60e+6 sec
55100 psi
@Temperature 1300 °F,
Time 1000 hour
 515 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
74700 psi
@Temperature 1200 °F,
Time 1000 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.7 µm/m-°C
@Temperature 93.0 °C
7.61 µin/in-°F
@Temperature 199 °F
Thermal Conductivity 12.6 W/m-K87.4 BTU-in/hr-ft²-°F
Melting Point 1220 - 1390 °C2230 - 2530 °F
Solidus 1220 °C2230 °F
Liquidus 1390 °C2530 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.75 - 1.3 %0.75 - 1.3 %
Boron, B 0.0080 - 0.016 %0.0080 - 0.016 %
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 14 - 16 %14 - 16 %
Iron, Fe 20.804 - 34.542 %20.804 - 34.542 %Balance
Manganese, Mn <= 0.75 %<= 0.75 %
Molybdenum, Mo 3.0 - 4.5 %3.0 - 4.5 %
Nickel, Ni 42 - 48 %42 - 48 %
Silicon, Si <= 0.75 %<= 0.75 %
Titanium, Ti 2.7 - 3.3 %2.7 - 3.3 %
Tungsten, W 3.0 - 4.5 %3.0 - 4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals UDIMET® Alloy 250 Maraging Steel
Astaras Anviloy® Weld Rod
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform

NINDA20 / 98911

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.