MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Sika Sikaflex® Mortar Fix One-component, polyurethane sealant
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Sikaflex Mortar Fix is a moisture-cured, 1-component, polyurethane-based, non-sag elastomeric sealant capable of ±25% joint movement. Meets Federal specification TT-S- 00230C, Type II. Meets ASTM C-920, Type S, Grade NS.

Where to Use:

  • Designed for all types of joints where maximum depth of sealant will not exceed ½ in.
  • Suitable for vertical and horizontal joints; readily placeable at 40°F (4°C).
  • Has many applications as an elastic sealant between materials with dissimilar coefficients of expansion.
  • Ideal for:
    • Weatherproofing of joints between brickwork, blockwork, masonry, concrete or metal frames.
    • Joints in walls, balconies, around window or door frames.
    • Expansion joints.
Advantages:
  • Excellent adhesion – bonds to most construction materials without a primer.
  • Textured appearance blends well to rough or stucco type surfaces.
  • Hides imperfections from tooling that a smooth sealant does not.
  • Excellent resistance to aging, weathering.
  • Non-staining.
  • Paintable with water-, oil- and rubber-based paints.
  • High elasticity – cures to a tough, durable, flexible consistency with exceptional cut and tear-resistance.
  • Stress relaxation.
  • Urethane-based; suggested by EPA for radon reduction.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 40
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 100 °CApplication Temp; Condition to room temp before low temp application.
Cure Time 168 hourFinal cure
Tack-Free Time <= 5.00 hour
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorLimestone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sika Sikaflex® Crack Flex Sealant High performance, textured, self-leveling, 1-part polyurethane sealant for sealing cracks.
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer
Taiwan PU Corporation UR50 Polyester Urethane Rubber
Mearthane Durethane™ S DS-245A Solid Polyurethane Elastomer
Mearthane Durethane™ S DS-230A Solid Polyurethane Elastomer

PSIKA928 / 209835

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.