MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyrocks Chemical 5003S2 Polypropylene, halogen-free flame retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: 5003S(+) is low halogen flame retardant PP with phosphorus, nitrogen and bromine as main flame retardant elements. It improves flame retardant efficiency by synergistic effect of solidifying phase and gas-phase mechanism, and accelerating melting and dripping by catalytic mechanism to play flame retardant performance. 5003S(+) flammability can reach UL94-V2(1.5mm and 3.0mm), glow-wire test meets GWIT 750? and GWFI 850?? 5003S(+) have UL certification, and meet the requirements of RoHS?SVHC?PFOS & PFOA?16P?Halogen-free?PAHs...etc. 5003S(+) has the characteristics of low smoke, low density of finished products, less corrosion to the mould etc

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Glow Wire Ignition Temperature 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
Pass; IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
Pass; IEC 60695-2-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROCKS016 / 278524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.