MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Hysol EA 9686 Film Adhesive
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Second generation, moisture resistant, toughened 250°F / 121°C curing film with service performance to 300°F / 149°C. Excellent for composite or metal bonding. Data from .060 psf, 300 g / m2.
    Applications:
  • Composite Bonding
  • Metal and Honeycomb Bonding
  • Composite Surfacing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 6.90 MPa1000 psiFlatwise
Adhesive Bond Strength  6.90 MPa
@Temperature 149 °C
1000 psi
@Temperature 300 °F
Lap Shear
 40.0 MPa
@Temperature -55.0 °C
5800 psi
@Temperature -67.0 °F
Lap Shear
 40.0 MPa
@Temperature 25.0 °C
5800 psi
@Temperature 77.0 °F
Lap Shear
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Glass Transition Temp, Tg 133 °C271 °Fdry
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 121 °C
1.00 hour
@Temperature 250 °F
 
Descriptive Properties
Honeycomb Climbing Drum Peel, mN/m76at 25°C
Out-Time (days)90at 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol EA 9313 Paste Adhesive System
Henkel Hysol EA 9330 Paste Adhesive System
3M Scotch-Weld™ DP-100 Epoxy Adhesive
3M Scotch-Weld™ DP 3501 Epoxy Adhesive
Henkel Hysol EA 934NA Paste Adhesive System

PHENK835 / 146840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.