MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite
Categories: Carbon; Graphite

Material Notes: Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminated with plastics, metals, adhesives, and other materials. Every SPREADERSHIELD™ part is customized to meet specific application needs and improve thermal performance within a limited space and weight. SPREADERSHIELD™ products have provided thermal solutions in a variety of industries and applications, including displays (PDP, LCD CCFL, LED BLU, OLED), cell phones, laptop and ruggedized computers, handheld gaming devices, batteries, projectors, set-top boxes, and automotive electronics. Each application is specialized to require different characteristics of SPREADERSHIELD™ products. Grade SS400 is designed specifically for large displays, notebook PCs, and handsets.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 51.0 micronsStandard
 76.0 micronsStandard
 127 micronsStandard
 250 micronsStandard
 380 micronsStandard
 430 micronsStandard
 510 micronsStandard
 50.0 - 1000 micronsAvailable Range
 940 micronsStandard
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9.70 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000520 ohm-cmIn-Plane
 0.0556 ohm-cmThrough-Plane
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.400 µm/m-°CIn-Plane
 27.0 µm/m-°CThrough-Plane
Specific Heat Capacity 0.700 J/g-°C
Thermal Conductivity 3.70 W/m-KNominal, Through-Plane; ASTM-D5470 Modified Method
 400 W/m-KNominal, In-Plane; Angstrom's Method
Maximum Service Temperature, Air 400 °C
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
 
Descriptive Properties
Thermal Contact Impedance - Per Side (°C·cm²/W)0.38at 0.50 mm spreader thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A283 Steel, grade D
JIS S45C Steel, Normalized
NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
ASTM A36 Steel, plate
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material

CGRAF902 / 107306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.