MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 82 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 82 is a light-fast citric acid ester plasticizer and solvent exhibiting a good compatibility with a wide range of polymers and resins, including cellulosics, polyvinyl acetate and polylactide

Chemical composition: Acetyl Triethyl Citrate (ATEC)

General properties and Applications: Uniplex 82 is characterized by a good compatibility with a large number of polymers such as cellulosics [like cellulose acetate (films, fibers), cellulose acetate butyrate, ethyl-cellulose, nitrocellulose], polyvinyl acetate, polyvinylchloride and polylactides. Uniplex 82 is used as a plasticizer and solvent in printing inks and in cosmetic products including nail lacquer and polish and hairstyling compositions. Uniplex 82 is a plasticizer developed for use in sensitive applications. Uniplex 82 is used when US regulations and recommendations governing food contacting applications need to be met.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.137 g/ccRelative
Brookfield Viscosity 54 cP
 
Thermal PropertiesOriginal ValueComments
Pour Point -40.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.436
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.25 %Karl Fischer
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceclear liquid
Color<50Hazen
Specifications<0.02%Acidity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9096 / 209487

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.