Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight Additive: Flame Retardant Features: Flame Retardant UL File Number: E157318 Processing Method: Injection Molding Information provided by TP Composites, Inc. |