MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPa
@Temperature 150 °C
 155 MPa
@Temperature 120 °C
 180 MPa
@Temperature 90.0 °C
 200 MPa
@Temperature 60.0 °C
 225 MPa
@Temperature 23.0 °C
Elongation at Break 1.5 %
@Temperature 23.0 °C
 1.7 %
@Temperature 60.0 °C
 1.7 %
@Temperature 90.0 °C
 2.0 %
@Temperature 120 °C
 2.5 %
@Temperature 150 °C
Tensile Modulus 15400 MPa
@Temperature 150 °C
 19000 MPa
@Temperature 120 °C
 20500 MPa
@Temperature 90.0 °C
 20600 MPa
@Temperature 60.0 °C
 21600 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 45.0 kJ/m²
Charpy Impact, Notched 6.50 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 235 °C
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C
Vicat Softening Point >= 300 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 370 - 400 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 2000 CF30 PEEK
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
Evonik VESTAKEEP® 2000 FC30 PEEK
Akro-Plastic Akrotek® PEEK CF 40 9 black (5182) PEEK, Conditioned, 40% Carbon Filled
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced

PLATH9647 / 177343

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.