MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Hifax™ RTA3263EC/1 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ RTA3263EC/1 fractional melt flow, 1,700 MPa flexural modulus, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact strength and processability. It was designed primarily for extruded automotive exterior profile applications. Uses: Automotive exterior parts, profiles

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ASTM D2240
Tensile Strength, Yield 23.0 MPa3340 psiASTM D 638
Elongation at Break 450 %450 %ASTM D 638
Flexural Modulus 1.50 GPa218 ksiTangent, 0.05 in/min; ASTM D790
 1.70 GPa247 ksiTangent, 0.5 in/min; ASTM D790
Izod Impact, Notched 7.400 J/cm13.86 ft-lb/in73°F; ASTM D256
Gardner Impact 32.0 J
@Temperature -30.0 °C
23.6 ft-lb
@Temperature -22.0 °F
ASTM D3029
Tear Strength 140 kN/m800 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
CTE, linear 47.0 µm/m-°C
@Temperature -30.0 - 100 °C
26.1 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C136 °FUnannealed; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMO801 / 53790

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.