MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sipol Technipol® Bio 1120 Aliphatic Copolyester
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description: TECHNIPOL® Bio 1120 is an aliphatic co-polyester, characterized a low melting point. Due to its formulation, it can be used in biodegradable and compostable compounds. Furthermore, it exhibits a good compatibility with other biodegradable polymers as polylactic acid and starch. It can be used as support polymer for master-batches both in granules and in powder form. Usable for injection molding.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D 792
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
MI 08
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161instantaneous; ASTM D 2240
Tensile Strength at Break 50.0 MPa7250 psiASTM D 638
Elongation at Break 450 %450 %ASTM D 638
Flexural Modulus 0.450 GPa65.3 ksiASTM D 638
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL040 / 297165

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.