MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Waspaloy B Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Waspaloy A has a higher solution temperature and longer time at stabilization than Waspaloy B. Typical Application: Jet engine discs

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  248 MPa
@Temperature 816 °C,
Time 360000 sec
36000 psi
@Temperature 1500 °F,
Time 100 hour
 696 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
101000 psi
@Temperature 1200 °F,
Time 1000 hour
 772 MPa
@Temperature 649 °C,
Time 360000 sec
112000 psi
@Temperature 1200 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.4 %1.4 %
Boron, B 0.0060 %0.0060 %
Carbon, C 0.070 %0.070 %
Chromium, Cr 19.5 %19.5 %
Cobalt, Co 13.5 %13.5 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 2.0 %<= 2.0 %
Manganese, Mn <= 0.75 %<= 0.75 %
Nickel, Ni >= 58.834 %>= 58.834 %As Balance
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.020 %<= 0.020 %
Titanium, Ti 3.0 %3.0 %
Zirconium, Zr 0.070 %0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Waspaloy A Nickel Superalloy (UNS N07001)
MetalTek WASPALOY® Centri-Vac Nickel Cobalt Based Alloy
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Special Metals NIMONIC® Alloy 80A

NZ97048 / 191447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.