MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 48571R006 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Side 1: Uncured Rubber
Side 2: Uncured Rubber

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness >= 1.00 milSide 1
 1.50 milPolyethylene Interleave
 >= 2.00 milSide 2
 2.50 milPrimed Coated 1080 Fiberglass (same as 108/no plied yarns), Substrate
 5.00 - 6.50 milOverall
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50Compound Property
Tensile Strength >= 800 psiCompound Property
Elongation at Break >= 550 %Compound Property
Peel Strength >= 6.00 pli[ppi], Bond Strength
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
UL RTI, Electrical 220 °Cper UL Card E54153
UL RTI, Mechanical without Impact 200 °Cper UL Card E54153
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 232 °C
Recommended Postcure Cycle
 15.0 min
@Temperature 177 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature <=23.9 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)4.5 - 5.5
Uncoated Fabric Break Strength40 lb/inFill Direction, Substrate Property
 70 lb/inWarp Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Rogers Arlon R32861R006 0.0055" (0.140 mm) Uncured Rubber with Fiberglass Substrate
Rogers Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate

PARL238 / 125424

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.