Chemical description: Preparation of various siloxanes. Application fields: GETREN® P 3300 is used as a sliding polymer for the coating of rubber seals to improve the sliding properties. GETREN® P 3300 was designed to facilitate the assembly of building and window profiles. Advantages: - The tempered film is stable on the surface of the profile.
- Migration of the sliding polymer into the rubber does not occur.
- GETREN® P 3300 forms a hydrophobic protective coating.
- GETREN® P 3300 improves the color strength of the rubber profile.
- In cases that coated seals come into contact with acrylic or polycarbonate glass, stress cracks will be avoided.
Information provided by Evonik |