Notes: Monprene OM-12260 is designed for overmolding applications for consumer industry. Monprene OM-12260 is an opaque grade that exhibits excellent adhesion to PC, ABS and PC/ABS. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Bondability; Lubricated; Medium Flow; Medium Density; Medium Hardness; Slip; Sunlight Resistant; UV Absorbing; Without Fillers Uses: Appliances; Bonding; Cell Phones; Dental Applications; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Sporting Goods; Toothbrush Handles; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |