MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Momentive Performance Materials GE Silicones Optic 3101 Translucent Silicone Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: GE Optic 3101 translucent silicone coating is a low VOC 100% silicone elastomeric coating used to provide a waterproof barrier to above grade surfaces. Optic coating cures to a durable, flexible and weatherproof membrane that is translucent for visual aesthetics.

Features: Silicone Durability, Waterproof Power, Low VOC, Vapor Permeable, Design Aesthetics, Light Transmission, Anti-Graffiti.

Applications: Brick, natural stones, and other surfaces where significant appearance change is undesirable. Glass block walls, skylights, stained glass windows, day lighting features, shelters, and other substrates through which light transmission is required. Applications requiring anti-graffiti performance.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccWPSTM P15
Solids Content 70 %70 %By weight.; WPSTM C19
 73 %73 %By volume.; WPSTM C19
Volatile Organic Compounds (VOC) Content <= 24 g/l<= 24 g/lEPA Method 24
Viscosity 12300 cP12300 cPWPSTM C-560
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2323ASTM D2240
Tensile Strength 0.834 MPa121 psiASTM D412
Elongation at Break 199 %199 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Optical PropertiesMetricEnglishComments
Gloss 27 %27 %Glossmeter
Transmission, Visible 95 %95 %10 mil DFT.; Color i7
 
Processing PropertiesMetricEnglishComments
Processing Temperature -6.67 - 48.9 °C20.0 - 120 °FApplication Temperature
Tack-Free Time 60.0 - 120 min1.00 - 2.00 hour
 
Descriptive Properties
Coverage Rate117 ft2/gal max
Resistance to Wind Driven RainpassASTM D6904
Skin Over Time< 30 minutes
Water Vapor Permeance18 permsASTM E96, wet cup. (10 mils DFT)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9911 / 265720

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.