System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Brass
Material Notes:
Copper-Zinc-Lead Alloy (Leaded Brass)
Finished product available as bar, wire, rod or shapes.
Chicago Extruded Metal temper codes: H01, H02
Information provided by Chicago Extruded Metals
Key Words:
ASM 4610, ASTM B16, SAE J461, SAE J463
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.307
lb/in³
Mechanical Properties
Original Value
Comments
Hardness, Rockwell B
22 - 80
Tensile Strength
40.0
-
80.0
ksi
Tensile Strength, Yield
15.0
-
45.0
ksi
Elongation at Break
4.0 - 50 %
Machinability
100 %
UNS C36000 (free-cutting brass) = 100%
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.00000663
ohm-cm
Thermal Properties
Original Value
Comments
Thermal Conductivity
804
BTU-in/hr-ft²-°F
Component Elements Properties
Original Value
Comments
Copper, Cu
60 - 63 %
Iron, Fe
0.35 %
Lead, Pb
3.1 - 3.7 %
Other, total
0.50 %
Zinc, Zn
32.45 - 36.05 %
as balance
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Mueller Alloy 3600 Free Cutting Brass (UNS C36000)
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy
AISI 12L13 Steel, cold drawn, 19-38 mm round
NCHICA912 / 147631
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.