MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® ABS Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Components: Acrylonitrile Butadiene Styrene based filament for Fused Filament Fabrication.

Product Description: ABS is the second most used 3D printing material. It is strong, flexible and has a high heat resistance. ABS is a preferred plastic for engineers and professional applications. ABS can be smoothened with acetone. To make a proper 3D print with ABS you will need a heated print bed. The filament is available in 9 colors.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³Printed Part; ISO 1183-1
Melt Flow 25.168 g/10 min
@Load 5.00 kg,
Temperature 220 °C
25.168 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 21.3 MPa3090 psiZX: Upright; ISO 527
 36.3 MPa5260 psiXY: Flat; ISO 527
Elongation at Break 1.8 %1.8 %ZX: Upright; ISO 527
 7.4 %7.4 %XY: Flat; ISO 527
Modulus of Elasticity 1.608 GPa233.2 ksiYoung's, ZX: Upright; ISO 527
 1.958 GPa284.0 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 38.59 MPa5597 psiZX: Upright; ISO 178
 56.6 MPa8210 psiXY: Flat; ISO 178
 58.3 MPa8460 psiXZ: On its edge; ISO 178
Flexural Modulus 1.586 GPa230.0 ksiZX: Upright; ISO 178
 1.767 GPa256.3 ksiXZ: On its edge; ISO 178
 1.833 GPa265.9 ksiXY: Flat; ISO 178
Flexural Strain at Break 3.1 %3.1 %ZX: Upright; ISO 178
 5.0 %5.0 %XZ: On its edge; ISO 178
 5.3 %5.3 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²ZX: Upright; ISO 180
 18.8 kJ/m²8.95 ft-lb/in²XY: Flat; ISO 180
 18.9 kJ/m²8.99 ft-lb/in²XZ: On its edge; ISO 180
Izod Impact, Unnotched (ISO) 7.20 kJ/m²3.43 ft-lb/in²ZX: Upright; ISO 180
 35.7 kJ/m²17.0 ft-lb/in²XZ: On its edge; ISO 180
 40.0 kJ/m²19.0 ft-lb/in²XY: Flat; ISO 180
Charpy Impact Unnotched 0.680 J/cm²3.24 ft-lb/in²ZX: Upright; ISO 179-2
 3.64 J/cm²17.3 ft-lb/in²XY: Flat; ISO 179-2
 4.22 J/cm²20.1 ft-lb/in²XZ: On its edge; ISO 179-2
Charpy Impact, Notched 0.280 J/cm²1.33 ft-lb/in²ZX: Upright; ISO 179-2
 1.60 J/cm²7.61 ft-lb/in²XY: Flat; ISO 179-2
 1.74 J/cm²8.28 ft-lb/in²XZ: On its edge; ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °FISO 75-2
Glass Transition Temp, Tg 104 °C219 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 90.0 - 110 °C194 - 230 °FBed, Bed Material: Glass
Nozzle Temperature 240 - 260 °C464 - 500 °F
Drying Temperature 60.0 °C140 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed40-80 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D001 / 312242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.