RT505F has good electrical properties under humid conditions and has excellent arc resistance. The “F” version is made from a fine weave fabric. Typical applications include fuse tubes and naval switchboard insulation. RT505F also complies with MIL-I-24768/8, Type GMG and ASTM D709 Type IV Grade G-5. Property data for 0.750" X 1.000" samples. Information provided by Norplex-Micarta |
Fiber Glass, Micarta, Melamine, NEMA G-5, MIL-I-24768/8 Type GMG, ASTM D709 Type IV Grade G-5 |