MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow 5A15H Polypropylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: DOW 5A15H is intended for use in injection molding processes and is particularly suited for applications requiring heat resistance. It complies with U.S. FDA 21 CFR 177.1520 (c)1.1a.

Information provided by Dow

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Temperature 230 °C
5.0 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5070 psimolded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 8.0 %8.0 %molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus, 1% Secant 1590 MPa230000 psimolded and tested per ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.374 J/cm0.700 ft-lb/inmolded and tested in accordance with ASTM D 4101; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °Funannealed; molded and tested in accordance with ASTM D 4101; ASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL TIMREX® PP 10 Natural Flake Graphite
BASF Novolen® 2340 P Polypropylene
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade
BASF Novolen® 1040 K Polypropylene
Covestro Baypreg® F 200 Polyurethane, Glass Mat Reinforced Sandwich

PDOW1227 / 30445

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.