Product Description: LLH100 is a linear low density polyethylene grade for applications that require high strength and toughness. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. This resin offers enhanced film strength, drawdown, toughness and heat seal strength. In addition this resin has excellent low temperature resistance for applications such as stretch film and frozen food packaging. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America Additive: Additive: Antiblock: No; Slip: No Features: Good Drawdown; Good heat Seal; High Strength; High Toughness; Low Temperature Resistance Uses: Bags; Food Packaging; Heavy-duty Bags; Liners; Packaging Processing Method: Extrusion Information provided by Osterman & Company |