MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ashley Polymers Ashlene® R6043 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Medium viscosity extrusion grade Nylon 6 resin with excellent melt stability, good melt strength: suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughness, resistance to abrasion; doesn't absorb food odors

Data provided by the manufacturer

Key Words: Polyamide 6; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Apparent Bulk Density 0.650 g/cc0.0235 lb/in³ASTM D1895
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 82.8 MPa12000 psiATSM D638
Tensile Strength, Yield 82.8 MPa12000 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature 249 - 260 °C480 - 500 °Fat die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNAA94 / 54441

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.