MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Redwood Plastics Redco™ FRP GRATING
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 - 1.94 g/cc0.0621 - 0.0701 lb/in³ASTM D792
Water Absorption 0.45 %
@Time 86400 sec
0.45 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4545ASTM D2583
Tensile Strength 48.3 MPa7000 psiCW; ASTM D638
 207 MPa30000 psiLW; ASTM D638
Modulus of Elasticity 19.3 GPa2800 ksi
Tensile Modulus 5.52 GPa800 ksiCW; ASTM D638
 17.2 GPa2500 ksiLW; ASTM D638
Flexural Strength 68.9 MPa10000 psiCW; ASTM D790
 207 MPa30000 psiLW; ASTM D790
Flexural Modulus 5.52 GPa800 ksiCW; ASTM D790
 12.4 GPa1800 ksiLW; ASTM D790
Compressive Strength 103 MPa15000 psiCW; ASTM D695
 207 MPa30000 psiLW; ASTM D695
Compressive Modulus 0.689 GPa100 ksiCW; ASTM D695
 17.2 GPa2500 ksiLW; ASTM D695
Shear Modulus 3.10 GPa450 ksi
Shear Strength 31.0 MPa4500 psiShort Beam; ASTM D-2344
 68.9 MPa10000 psiPunch; ASTM D-732
Izod Impact, Notched 2.16 J/cm4.05 ft-lb/inCW; ASTM D256
 13.5 J/cm25.3 ft-lb/inLW; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.0
@Frequency 60 Hz
5.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 7.87 kV/mm200 kV/inASTM D149
Arc Resistance 120 sec120 secLW; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C4.44 µin/in-°FASTM D696

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW122 / 296688

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.