MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics THERMATTACH® T410 Thermally Conductive Attachment Tape
Categories: Polymer; Tape

Material Notes: Description: Chomerics’ patented THERMATTACH® T410 double-sided adhesive tape provides and effective thermal interface and heat sink attachment method for plastic component packages. The tape is thermally conductive and has exceptional bonding properties. It can also be used to adhere components to vertical heat sinks or to metal chassis walls in place of clips, crews or other mechanical fasteners, without the need for additional thermal compounds. THERMATTACH® t410 tape can be applied directly to the silicone mold release-contaminated package surface without using primers. THERMATTACH® T410 tape can be consistently applied to meet the thermal and adhesive requirements of most designs.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 140 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6063 psiASTM D412
Adhesive Bond Strength 0.276 MPaDie Shear Adhesion; Steel/FR4 at 125°C; Chomerics #54
 0.437 MPaDie Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; Control
 1.05 MPaDie Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; Control
 1.172 MPaLap Shear Adhesion; ASTM D1002
 1.172 MPaDie Shear Adhesion; Steel/FR4 at 25°C; Chomerics #54
 0.145 MPa
@Temperature 150 °C
Die Shear Adhesion; Steel/FR4
 0.276 MPa
@Temperature 125 °C
Die Shear Adhesion; Steel/FR4
 1.19 MPa
@Temperature 25.0 °C
Die Shear Adhesion; Steel/FR4
 0.171 MPa
@Load 11.3 kg
Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; Control; ASTM D1000
 0.414 MPa
@Load 0.907 - 2.27 kg
Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; Control; ASTM D1000
 0.807 MPa
@Load 76.2 kg,
Temperature 125 °C
Die Shear Adhesion; FR4/Al
 0.808 MPa
@Load 0.907 - 2.27 kg,
Temperature 125 °C
Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; 1000 hrs; Heat Age; ASTM D1000
 0.910 MPa
@Load 0.907 - 2.27 kg,
Temperature 85.0 °C
95%; Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; 1000 hrs; High Temp/ Humidity Resist; ASTM D1000
 2.32 MPa
@Load 76.2 kg,
Temperature 25.0 °C
Die Shear Adhesion; FR4/Al
 1.40 MPa
@Temperature 125 °C,
Time 3.60e+6 sec
Die Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; Heat Age
 2.64 MPa
@Temperature 85.0 °C,
Time 3.60e+6 sec
Die Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; High Temp/ Humidity Resist.
 1.45 MPa
@Treatment Temp. 50.0 - 100 °C,
# of Cycles 25.0
Die Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; Thermal Shock
 1.67 MPa
@Treatment Temp. 25.0 - 125 °C,
# of Cycles 1000
Die Shear Adhesion; Applied to 80386 PQFP packages; .5" x .5" sample; Temp Cycling
 0.503 MPa
@Load 0.907 - 2.27 kg,
Treatment Temp. 50.0 - 100 °C
Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; 25 cycles; Thermal Shock; ASTM D1000
 0.867 MPa
@Load 0.907 - 2.27 kg,
Treatment Temp. 25.0 - 125 °C
Die Shear Adhesion; FR4 to 2024 Aluminum; 1" x 5" sample; 1000 cycles; Temp Cycling; ASTM D1000
Tear Strength 390 pliASTM D624
Peel Strength 0.587 kN/m90°; Average; 2" x.55" sample; Control
 1.23 kN/m180°; ASTM D1000
 0.438 kN/m
@Treatment Temp. 85.0 °C,
Time 3.60e+6 sec
95% RH; 90°; Average; 2" x.55" sample; High Temp/ Humidity Resist.
 0.543 kN/m
@Treatment Temp. 125 °C,
Time 3.60e+6 sec
90°; Average; 2" x.55" sample; Heat Age
 0.438 kN/m
@Treatment Temp. 50.0 - 100 °C,
# of Cycles 25.0
90°; Average; 2" x.55" sample; Thermal Shock
 0.587 kN/m
@Treatment Temp. 25.0 - 125 °C,
# of Cycles 1000
90°; Average; 2" x.55" sample; Temp. Cycles
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.250 W/m-KASTM D5470
 
Descriptive Properties
CarrierAluminum
ColorClear/White
Creep Adhesion150°C and 12 psi load; PSTC-7
 25°C and 12 psi load; PSTC-7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4028 Steel
Aluminum 2024-T6
Alclad Aluminum 7075-T6, T651
Misumi ANP79 Aluminum Alloy
Aluminum A535.0-F or Aluminum 535.0-T5, Cast

PCHOME354 / 131064

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.