MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ResMart Ultra POM 9
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: High Performance Copolymer Polyacetal

Information provided by ResMart

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Linear Mold Shrinkage 0.020 in/inASTM D955
Melt Flow 9.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9300 psiASTM D638
Tensile Modulus 400000 psiASTM D638
Flexural Strength 12600 psiASTM D790
Flexural Modulus 370000 psiASTM D790
Izod Impact, Notched 1.20 ft-lb/inASTM D256
Izod Impact, Unnotched 2.90 ft-lb/inISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 316 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 214 °FUnannealed; ASTM D648
Vicat Softening Point 161 °FISO 306
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 - 400 °F
Mold Temperature 140 - 175 °F
Drying Temperature 210 - 230 °F
Dry Time 3.00 - 4.00 hour
Injection Pressure 7500 - 15000 psi
 
Descriptive Properties
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRSMRT050 / 280688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.