MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CHT QVB 720 Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a pourable 2-part addition cure silicone elastomer system. After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at ambient temperatures within 24 hours, but the rate of cure can be accelerated by heat. The cured rubber exhibits excellent physical and electrical properties.

Key Features

  • Transparent purple in thin cured sections which enables layer thickness evaluation
  • Fast gel time
  • Excellent tear and elongation properties
  • Flowable, self-leveling and mildly thixotropic for vertical surfaces
Key Applications
  • Closed molding
  • Composite part manufacturing
  • Resin infusion/pre-preg
Application: QVB 720 is a silicone molding rubber for producing reusable vacuum bags. This formulation can also be used as a mold making material if a fast cure is required.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccA; BS ISO 2781
 1.07 g/ccB; BS ISO 2781
 1.07 g/ccCured; BS ISO 2781
Brookfield Viscosity 35000 cPA
 35000 cPB
Linear Mold Shrinkage 0.0010 cm/cm
Storage Temperature <= 38.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 28ASTM D 2240-95
Tensile Strength 700 psiISO 37
Elongation at Break 800 %ISO 37
Tear Strength 60.0 pliBS ISO 34-1
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
ColorTranslucent purpleB
 Translucent purpleCured Product
 Translucent whiteA
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL154 / 314637

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.