MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SunChemical Gwent C2100217D1 Aluminium for PTC paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Aluminium Ink designed to give good ohmic contact on to barium titanate PTC components. This product is particularly good where large volumes of PTC components are being processed in belt furnaces conditions, where improved stain resistance and good visual appearance are required.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester
Substrate: PTC ceramic parts

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 68 - 72 %
@Temperature 150 °C
68 - 72 %
@Temperature 302 °F
Viscosity 11000 - 18000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
11000 - 18000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 780 - 910 °C1440 - 1670 °F
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g227Using a 230 mesh stainless steel screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Elements Barium Titanate nanoparticles
SunChemical Gwent C2030217D2 Aluminium for PTC paste
Harris Acoustic Sensors EC-21 Barium Titanate Piezoelectric
Barium Titanate, BaTiO3
Channel Industries 300 Barium Titanate Piezoelectric

WGELZ9066 / 139379

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.