MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® Pipe Sealer TORQUE 176 Anaerobic Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TORQUE 176 is a medium strength anaerobic adhesive for sealing hydraulic and pneumatic threads connectors up to 2”. To replace PTFE tapes in the sealing of gases, water, LPG, hydrocarbons, oils and other chemicals. TORQUE 176 is medium thixotropic which prevents migration of the sealant before or during curing. Highly resistant to heat, corrosion, shocks and vibrations.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 20000 cP20000 cP
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 8.00 - 12.0 MPa1160 - 1740 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 100 °C>= 212 °Funcured
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 - 30.0 min0.250 - 0.500 hourhandling
 60.0 - 180 min1.00 - 3.00 hourfunctional
 300 - 600 min5.00 - 10.0 hourfull
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
Color / appearanceblue
Locking Torque10-15 Nm, breakaway
 12-18 N., prevailing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9189 / 233555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.