Description: Vacuum bagging film. Ideally suited to aerospace applications. Features & Benefits: - Heat stabilized vacuum bagging film with a high elongation
- Suitable for high temperature autoclave curing of aerospace composites, including BMIs for cure temperatures up to 215°C/419°F
- Recommended for bagging applications where a higher softness is required
- Not recommended for use with phenolic resins or strong oxidizer.
Information provided by Cytec, subsequently acquired by Solvay. |