MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber for low to high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Filler Content 30 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 228 MPaASTM D638
Elongation at Break 4.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 331 MPaASTM D790
Flexural Modulus 17200 MPaASTM D790
Izod Impact, Notched 80.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.0 - 1000 ohm-cmASTM D257
Surface Resistance 1.0 - 1000 ohmASTM D257
 
Processing PropertiesOriginal ValueComments
Melt Temperature 282 - 310 °C
Mold Temperature 93.3 - 107 °C
Drying Temperature 71.1 - 82.2 °C
 
Descriptive Properties
FeaturesGood Chemical Resistance
 High Stiffness
 Semi Crystalline
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Business Equipment
 Computer Components
 Connectors
 Electrical/Electronic Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Avient OnColor™ 30BKA488 Black Polyvinyl Chloride
Avient Lubri-Tech™ PC-40CF/15T Polycarbonate (PC), Carbon Fiber Reinforced, PTFE Lubricated
Avient Lubri-Tech™ PC-30CF/15T Polycarbonate (PC)
Avient Lubri-Tech™ PC-30CF/15T FR V0 Polycarbonate (PC), Carbon Fiber Reinforced, PTFE Lubricated

PH0POL1125 / 145694

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.