MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CoorsTek YTZP Yttria Partially Stabilized Zirconia, Hipped
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.

Data Provided by the manufacturer, CoorsTek, Inc.

Key Words: ZrO2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.07 g/cc0.219 lb/in³ASTM C20
Water Absorption 0.00 %0.00 %ASTM 373
Particle Size 1.0 µm1.0 µmThin Section Crystal Size
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 12.712.71000 g
Hardness, Rockwell 45 N 8181
Modulus of Elasticity 210 GPa30500 ksiASTM C848
Flexural Strength 1720 MPa249000 psiASTM F417
Compressive Strength 2500 MPa363000 psiASTM C773
Poissons Ratio 0.230.23ASTM C848
Fracture Toughness 13.0 MPa-m½11.8 ksi-in½Notched Beam
Shear Modulus 85.0 GPa12300 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmASTM D1829
 <= 1000 ohm-cm
@Temperature 1000 °C
<= 1000 ohm-cm
@Temperature 1830 °F
ASTM D1829
 20000 ohm-cm
@Temperature 500 °C
20000 ohm-cm
@Temperature 932 °F
ASTM D1829
Dielectric Constant 29
@Frequency 1e+6 Hz
29
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 9.00 kV/mm229 kV/inAC; ASTM D116
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.3 µm/m-°C
@Temperature 25.0 - 1000 °C
5.72 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°FASTM E1269
Thermal Conductivity 2.20 W/m-K15.3 BTU-in/hr-ft²-°FASTM C408
Maximum Service Temperature, Air 1500 °C2730 °FNo Load
 
Descriptive Properties
ColorIvory

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
China-Yixing Longly Refractories Zirconia Ceramics
ICE ZrO
Overview of materials for Nylon 12
Steatite (Magnesium Silicon Oxide)

CZ3CAA / 2754

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.