MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPV 3135 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3100 series are engineered materials designed primarily general purpose, automotive and industrial applications requiring a good balance of thermal, mechanical, and physical properties. Sarlink 3135, available in NAT and BLK, is a low hardness, low density, multi-purpose thermoplastic vulcanizate that can be processed by injection molding, blow molding or extrusion for applications such as grips, seals, gaskets, profiles, hose & tubes, bellows, and other articles.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Bondability; Chemical Resistant; General Purpose; Good Adhesion; Good Flexibility; Good Moldability; Good Processability; Good Surface Finish; High Elasticity; High Heat Resistance; High Melt Stability; Low Density; Low Hardness; Low Specific Gravity; Resilient

Uses: Appliance Components; Automotive Applications; Automotive Exterior Parts; Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Gaskets; General Purpose; Handles; Industrial Applications; O-rings; Pipe Seals; Plugs; Profiles; Rubber Replacement; Seals

RoHS Compliance: RoHS Compliant

Agency Ratings: UL 94

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 g/cc0.0337 lb/in³ASTM D792
Viscosity 270 cP
@Shear Rate 206 1/s,
Temperature 200 °C
270 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  38
@Time 5.00 sec
38
@Time 0.00139 hour
Extruded; ISO 868
 42
@Time 5.00 sec
42
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 2.20 MPa319 psiFlow; ISO 37
 4.00 MPa580 psiAcross Flow; ISO 37
 4.00 MPa
@Treatment Temp. 135 °C,
Time 360000 sec
580 psi
@Treatment Temp. 275 °F,
Time 100 hour
Across Flow, Change in Air; ISO 188
 4.16 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
603 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
Across Flow; ISO 37
 2.10 MPa
@Strain 100 %
305 psi
@Strain 100 %
Flow; ISO 37
 1.15 MPa
@Strain 100 %,
Treatment Temp. 135 °C
166 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air, 1000 hr; ISO 188
 1.22 MPa
@Strain 100 %,
Treatment Temp. 150 °C
178 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air, 168 hr; ISO 188
Elongation at Break 200 %200 %Flow; ISO 37
 600 %600 %Across Flow; ISO 37
 206 %
@Treatment Temp. 150 °C,
Time 605000 sec
206 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 588 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
588 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 15.1 kN/m86.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  15 %
@Temperature 22.8 °C,
Time 79200 sec
15 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 52 %
@Temperature 90.0 °C,
Time 252000 sec
52 %
@Temperature 194 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 216 °C350 - 420 °FInjection, Melt
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 177 - 216 °C350 - 420 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Back Pressure 0.0689 - 0.345 MPa10.0 - 50.0 psiInjection
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui Milastomer™ 4010NS Natural Vulcanized Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer
ExxonMobil Dytron™ XK7300-92 Thermoplastic Elastomer

PTEKNQ1137 / 237628

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.