MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos J50-1000-178 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: A high density polyethylene copolymer intended for the injection molding of closures for beverages. Because of its high purity and excellent organoleptic properties, this grade is certified as low taste and is intended for packaging in direct contact with beverages. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Designed for injection molding of screw caps and specialty food containers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccASTM D4883
Environmental Stress Crack Resistance 4.0 hourASTM D 1693A
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 25.5 MPa2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 500 %2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.207 GPaTangent; ASTM D 790
Izod Impact, Notched 0.500 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °CASTM D648
Vicat Softening Point 128 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® H5656 High Density Polyethylene, Injection Molding Grade
Ineos J50-1000-187 HDPE
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin

PSOLKA / 68217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.