MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel 416R Chromium Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific requirements ( HRC 24/28, 28/32, or 32/36). Crucible 416R was specifically designed by Crucible engineers in collaboration with barrel makers and rifle manufacturers to provide consistency, high quality and the following characteristics:
  • Good machinability for gun drilling and reaming, plus excellent polishability for uniform lapping, necessary for bore accuracy.
  • A homogeneous microstructure which responds to heat treat providing a uniform hardness along the length of the bar, necessary for accurate button rifling to precise groove dimensions.
  • An optimum combination of high tensile strength along with adequate toughness to withstand the typical chamber pressures encountered during firing.
  • Good corrosion resistance to inhibit rusting and which also helps to minimize fouling. Crucible 416R provides a durable finish which does not pit when properly maintained.
  • Precision straightened and stress relieved bars, either mill length or multi length, ready to be cut to length and gun drilled.
  • 100% ultrasonic testing for reliable barrels.
  • Crucible 416R stainless steel is manufactured using very stringent controls from initial melting, through hot rolling, heat treating, cold finishing and final bar inspection. Barrels made from Crucible 416R are used at all levels of competition and in all conditions dry, damp or salty. Although all martensitic stainless steels have reduced ductility at very low temperatures, Crucible 416R can be safely used down to minus 40°F (-40°C).

    Information provided by Crucible Specialty Metals.

    Key Words: Precision Rifle Barrel Stock
    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.75 g/cc0.280 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Brinell 170170
    Hardness, Rockwell C 28 - 3628 - 36
    Tensile Modulus 200 GPa29000 ksi
    Poissons Ratio 0.380.38Calculated
    Shear Modulus 72.3 GPa10500 ksi
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  9.90 µm/m-°C
    @Temperature -6.00 - 100 °C
    5.50 µin/in-°F
    @Temperature 21.2 - 212 °F
     10.1 µm/m-°C
    @Temperature 0.000 - 315 °C
    5.61 µin/in-°F
    @Temperature 32.0 - 599 °F
     11.5 µm/m-°C
    @Temperature 0.000 - 538 °C
    6.39 µin/in-°F
    @Temperature 32.0 - 1000 °F
    Specific Heat Capacity 0.460 J/g-°C
    @Temperature 0.000 - 100 °C
    0.110 BTU/lb-°F
    @Temperature 32.0 - 212 °F
    Thermal Conductivity  25.1 W/m-K
    @Temperature 93.0 °C
    174 BTU-in/hr-ft²-°F
    @Temperature 199 °F
     28.5 W/m-K
    @Temperature 538 °C
    198 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.12 %0.12 %
    Chromium, Cr 12.5 %12.5 %
    Iron, Fe 86.05 %86.05 %As Remainder
    Manganese, Mn 0.40 %0.40 %
    Molybdenum, Mo 0.40 %0.40 %
    Silicon, Si 0.40 %0.40 %
    Sulfur, S 0.13 %0.13 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    410 Stainless Steel
    420 Stainless Steel
    416 Stainless Steel
    416 Stainless Steel, tempered bar
    AISI 1211 Steel, cold drawn, 19-38 mm round

    NCRUC032 / 16025

    New MatWeb Services

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.