MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT Group QM Cat Thixo 2 Thixotropic, Condensation Cure Moldmaking Catalyst
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM Cat Thixo 2 is a thixotropic, two-component, room temperature, condensation cure catalyst for the QM 100 series of products. The catalyst exhibits non-slump behavior to ~ 0.5” while not changing the cured properties of the QM 100 series bases. Applications include glove molding, lay-up molding, spray applications or any application where a thixotropic moldmaking material is required. The cured rubber has excellent mechanical properties and good shelf-life stability. This technology is also available with QM Cat Purple.

Key Features:

  • Applicable bases include QM 113, QM 118, QM 122, QM 128, QM 135 and QM 140
  • Fast demold time
  • Non-slump range of ~ 0.25” – 0.5” depending on the QM 100 base used
Main Applications:
  • Spray applications
  • Lay-up molding
  • Glove molding applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccUncatalyzed, QM Cat Clear Thixo 2
 1.03 g/cc1.03 g/ccUncatalyzed, QM Cat Purple Thixo 2
 1.03 g/cc1.03 g/ccUncatalyzed, QM Cat Blue Thixo 2
Viscosity 1000 cP1000 cPCatalyzed, QM Cat Clear Thixo 2
 1000 cP1000 cPCatalyzed, QM Cat Purple Thixo 2
 1000 cP1000 cPCatalyzed, QM Cat Blue Thixo 2
 
Processing PropertiesMetricEnglishComments
Cure Time 720 - 960 min12.0 - 16.0 hourDemold time, Catalyzed, QM Cat Clear Thixo 2
 720 - 960 min12.0 - 16.0 hourDemold time, Catalyzed, QM Cat Purple Thixo 2
 960 - 1440 min16.0 - 24.0 hourDemold time, Catalyzed, QM Cat Blue Thixo 2
Tack-Free Time 240 - 360 min4.00 - 6.00 hourCatalyzed, QM Cat Clear Thixo 2
 240 - 360 min4.00 - 6.00 hourCatalyzed, QM Cat Purple Thixo 2
 360 - 480 min6.00 - 8.00 hourCatalyzed, QM Cat Blue Thixo 2
Pot Life 45.0 min45.0 minCatalyzed, QM Cat Clear Thixo 2
 45.0 min45.0 minCatalyzed, QM Cat Purple Thixo 2
 50.0 min50.0 minCatalyzed, QM Cat Blue Thixo 2
 
Descriptive Properties
ColorBeige/WhiteCatalyzed, QM Cat Clear Thixo 2
 BlueUncatalyzed, QM Cat Blue Thixo 2
 Light BlueCatalyzed, QM Cat Blue Thixo 2
 Light PurpleCatalyzed, QM Cat Purple Thixo 2
 PurpleUncatalyzed, QM Cat Purple Thixo 2
 TranslucentUncatalyzed, QM Cat Clear Thixo 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PACC2069 / 199457

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.