MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Poco Graphite AXM-5Q Industrial Grade Graphite
Categories: Carbon; Graphite

Material Notes: POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal graphite to each application. Post synthesis modifications enhance the original material to allow even greater flexibility for highly specialized conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 1.73 g/cc
Open Porosity 85 %
Porosity 23 %
Particle Size 5.0 µm
Pore Size 0.800 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72
Tensile Strength, Yield 48.0 MPa
Elongation at Yield 0.99 %
Modulus of Elasticity 10.5 GPa
Flexural Strength 69.0 MPa
Compressive Strength 124 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00165 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.80 µm/m-°C
Thermal Conductivity 88.0 W/m-K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Poco Graphite AXF-5Q Industrial Grade Graphite
Poco Graphite ZXF-5Q Industrial Grade Graphite
Poco Graphite AXZ-5Q Industrial Grade Graphite
Poco Graphite ACF-10Q Industrial Grade Graphite
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Stress Relieved

CPOCO11 / 85588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.