MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Aluminum 6013-T651
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: General 6013 characteristics and uses: High strength and good corrosion resistance. Easily joined by all welding and brazing methods. Excellent compressive properties. Uses include ABS Braking systems, hydraulic applications, valves, machine parts, roller blade parts, munitions.

Data supplied by Alcoa.

Key Words: 6013-T651 Aluminium; UNS A96013; Al6013-T651
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130130500 kg load/10 mm ball
Hardness, Knoop 163163Estimated from Brinell
Hardness, Rockwell A 49.549.5Estimated from Brinell
Hardness, Rockwell B 8080Estimated from Brinell
Hardness, Vickers 149149Estimated from Brinell
Tensile Strength, Ultimate >= 379 MPa>= 55000 psi
Tensile Strength, Yield >= 359 MPa>= 52100 psi
Elongation at Break >= 5 %>= 5 %
Machinability 70 %70 %0-100 Scale (A=90; B=70; C=50; D=30; E=10)
Shear Strength 248 MPa36000 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000490 ohm-cm0.00000490 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
average
Thermal Conductivity 164 W/m-K1140 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.8 - 97.8 %94.8 - 97.8 %As remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 0.60 - 1.1 %0.60 - 1.1 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 0.80 - 1.2 %0.80 - 1.2 %
Manganese, Mn 0.20 - 0.80 %0.20 - 0.80 %
Other, each <= 0.15 %<= 0.15 %
Other, total <= 0.050 %<= 0.050 %
Silicon, Si 0.60 - 1.0 %0.60 - 1.0 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.25 %<= 0.25 %
 
Descriptive Properties
Applied Coating AcceptanceGood
General Corrosion ResistanceBA = best; E = worst
MachinabilityGood
Stress Corrosion Cracking ResistanceAA = best; E = worst
WeldabilityAA = best; E = worst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6013-T8
Aluminum 6061-T6; 6061-T651
Alcoa Excalibar® 6013-T651 Aluminum
Aluminum 6005-T1
Aluminum 6020-T651

MA6013T651 / 133710

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.