MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Polystyrene Foam Insulation 78 Spray Adhesive
Categories: Polymer; Adhesive

Material Notes: A high strength, industrial grade spray adhesive that is typically used for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and extruded polystyrene foam.

Features:

  • Aggressively tacky industrial grade spray adhesive that is typically used for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and extruded polystyrene foam.
  • Will not dissolve polystyrene foam
  • High coverage product
  • Capable of both one a two surface bonding

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.755 g/cc0.0273 lb/in³Aerosol
 0.791 g/cc0.0286 lb/in³Bulk
Solids Content 19.1 %19.1 %Aerosol
 35 %35 %Bulk
Volatile Organic Compounds (VOC) Content 508 g/l508 g/l
Viscosity <= 500 cP<= 500 cPBulk
 
Descriptive Properties
AppearanceTranslucentAerosol
 TranslucentBulk
BaseSynthetic ElastomerAerosol
 Synthetic ElastomerBulk

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Styrofoam™ Ultra SL Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Scoreboard Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ SM Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Tongue and Groove Extruded Polystyrene Foam Insulation
Aluminum, Al

PMM34058 / 168805

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.