MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Unifrax FyreWrap® MAX 2.0 Duct Insulation Two-Layer ASTM E-2336 System
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Unifrax's FyreWrap® MAX 2.0 Duct Insulation is a high-temperature insulation blanket specifically designed to provide a flexible enclosure for one- and two-hour rated commercial kitchen grease ducts. FyreWrap MAX 2.0 Duct Insulation provides a tested, fire-protective enclosure acceptable as an alternate to a traditional fire-rated shaft. Installed as a two-layer system, FyreWrap MAX 2.0 complies with ICC ES Acceptance Criteria for Grease Duct Enclosure Assemblies, AC101 (formerly ICBO) and ASTM E-2336. FyreWrap MAX 2.0 Duct Insulation offers the following product freatures:

  • Complies with ASTM E-2336 and ICC ES criteria
  • Two-layer system; inner layer utilizes butt joint
  • High-temperature, biosoluble insulation
  • Zero clearance to combustible, at any location
  • 2-hour fire endurance rating
  • Alternate to shaft enclosure

    Product ComponentsCore Material: FyreWrap MAX 2.0 incorporates Insulfrax® Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from a calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket product form.
  • Encapsulating Material: The core insulation blanket is completely encapsulated in an aluminum foil fiberglass reinforced scrim covering. This scrim provices additional handling strength as well as protection from moisture absorption and tearing.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/ft³
Thickness 2000 mil
 
Descriptive Properties
ASTM C136 Non-combustibilityPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Thermal Ceramics Superwool 607 Max Pyro-Fold and Pyro-Stack Modules
Thermal Ceramics Superwool 607 Max 111 Bulk
Thermal Ceramics Kaowool 3000 Paper
Rogers Arlon DiClad 880 PTFE/Woven Fiberglass Laminate

CUNIF116 / 97888

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.