MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lucite International Elvacite® 2927 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Lucite International has developed novel polymer chemistry which delivers Elvacite® thermoplastic acrylic resins with controlled molecular architecture and enables the coatings formulator to achieve higher solids solutions / lower VOC emissions without significant compromise to physical properties or causing odor problems. The technology has been developed with a VOC limit target of 3.5 lb./gal.

Elvacite® 2927 can be employed in a wide range of inks and coatings systems, where the increased solids or reduced solution viscosity are desired. Typical applications include: Industrial Coatings, Concrete Coatings, Marine Paints, Solvent based Inks, UV Coatings and Inks.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
Viscosity Measurement 0.11 - 0.13Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 19000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 3.5
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 46.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.65 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Elvacite® 4400 Acrylic Resin
BYK Optiflo® T1000 (Formerly RXL-7301) Polymer
Blue River Coatings Acrylic 4000 Topcoat
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Mallard Creek Polymers Rovene® 6087 Styrene-Acrylic Emulsion

PLUCIT9470 / 150184

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.